DENTAL
Exaduro Pink
This type III dental stone has low expansion, is smooth and has highly resistant edges. It may be used for crown and bridge work, or chrome and cobalt work. It is also ideal for orthodontic antagonistic models.
MIXING
The plaster/ water ratio indicated below is recommended. The plaster is poured into the water (never the other way around), is allowed to moisten and is mixed for approximately one minute, stirring it gently and evenly to prevent the formation of air bubbles. The recipients must be clean.
STORAGE
In dry areas on wooden slats, with spaces between rows and with the wall to ensure free air circulation.
ANALYSIS
PHYSICAL SPECIFICATIONS
Colour: Pink
Mixing Rate: 357 gr plaster/ 100 gr water
Water Factor: 28 gr of water / 100 gr plaster (water/ plaster ratio used to obtain results of analysis)
Start setting time: Minimum 3 minutes
Finish Setting Time: 15 minutes
Setting Expansion: 1.2 mm / m
Linear Expansion: 0.1%
Compressive Strength: > 60 Mpa
Brinell Hardness: > 3000 kg / cm²
Exaduro White
Dental Stone Type III with low expansion indicated for the manufacture and removal of prostheses, resins, antagonist and strong ceramic models with high resistance edges.
See Exaduro White in this store
MIXING
The plaster/ water ratio indicated below is recommended. The plaster is poured into the water (never the other way around), is allowed to moisten and is mixed for approximately one minute, stirring it gently and evenly to prevent the formation of air bubbles. The recipients must be clean.
STORAGE
In dry areas on wooden slats, with spaces between rows and with the wall to ensure free air circulation.
ANALYSIS
PHYSICAL SPECIFICATIONS
Colour: White
Mixing Rate: 130 gr plaster / 100 gr water
Water Factor: 80 gr water / 100 gr plaster (water/ plaster ratio used to obtain results of analysis)
Start setting time: 4 – 5 minutes
Finish Setting Time: 18 – 20 minutes
Setting Expansion: 1.5 mm / m
Linear Expansion: 0.1%
Compressive Strength: > 60 Mpa
Brinell Hardness: > 3000 kg / cm²
Exaduro Yellow
Yellow plaster ideal for basing (Crown and Bridge work), working models, opposing models, acrylic restorations etc.
See Exaduro Yellow in this store
MIXING
The plaster/ water ratio indicated below is recommended. The plaster is poured into the water (never the other way around), is allowed to moisten and is mixed for approximately one minute, stirring it gently and evenly to prevent the formation of air bubbles. The recipients must be clean.
STORAGE
In dry areas on wooden slats, with spaces between rows and with the wall to ensure free air circulation.
ANALYSIS
PHYSICAL SPECIFICATIONS
Colour: Yellow
Mixing Ratio: 350 gr plaster / 100 gr water
Water Factor: 28 gr water / 100 gr plaster (water/ plaster ratio used to obtain results of analysis)
Start setting time: 4 – 5 minutes
Finish Setting Time: 13 – 15 minutes
Setting Expansion: 1.2 mm / m
Brinell Hardness: > 3000 kg / cm²